Specification | General PTFE thickness and negative pressure-resistance | The thickness of PTFE wall required to resist-0.1MPA pressure when the temperature is less than 120degree, | |
DN25 | 2mm | -0.08Mpa | 3mm(L≤3000mm) |
DN32 | 2mm | -0.075Mpa | 3mm(L≤3000mm) |
DN40 | 2.5mm | -0.075Mpa | 4mm(L≤3000mm) |
DN50 | 2.5mm | -0.06Mpa | 5mm(L≤3000mm) |
DN65 | 2.5mm | -0.05Mpa | 8mm(L≤1000mm) |
DN80 | 3mm | -0.05Mpa | 10mm(L≤1000mm) |
DN100 | 3mm | -0.04Mpa | 13mm(L≤1000mm) |
DN125 | 4mm | -0.03Mpa | 13mm(L≤1000mm) |
DN150 | 4mm | -0.025Mpa | 13mm(L≤1000mm) |
DN200 | 5mm | -0.02Mpa | 15mm(L≤1000mm) |
PTFE lined 90° elbow | Unit mm | ||||||||
Nominal diameter | Specification of balled iron T | Raised face A | Central height C1 | Inside diameter D1 | PTFE thickness | out side diameter of flange D | Diameter of bolt circle K | Thickness of flange C | |
DN(mm) | NPS(inch) | ||||||||
DN15 | 1/2 | 34 | 40 | 80 | 15 | 5 | 90 | 65 | 11 |
DN20 | 3/4 | 38 | 45 | 90 | 18 | 5 | 100 | 75 | 11 |
DN25 | 1 | 42 | 60 | 92 | 22 | 5 | 110 | 85 | 12 |
DN32 | 1 1/4 | 48 | 70 | 100 | 28 | 5 | 130 | 100 | 13 |
DN40 | 1 1/2 | 57 | 80 | 112 | 38 | 5 | 140 | 110 | 14 |
DN50 | 2 | 68 | 95 | 117 | 48 | 5 | 155 | 125 | 14 |
DN65 | 2 1/2 | 89 | 115 | 135 | 63 | 8 | 175 | 145 | 16 |
DN80 | 3 | 108 | 130 | 150 | 78 | 8 | 190 | 160 | 16 |
DN100 | 4 | 114 | 150 | 150 | 87 | 8 | 210 | 180 | 18 |
DN125 | 5 | 140 | 180 | 190 | 110 | 8 | 240 | 210 | 20 |
DN150 | 6 | 168 | 205 | 230 | 135 | 10 | 275 | 240 | 20 |
DN200 | 8 | 219 | 260 | 305 | 180 | 10 | 330 | 295 | 20 |
DN250 | 10 | 273 | 315 | 380 | 230 | 12 | 385 | 350 | 23 |
DN300 | 12 | 325 | 365 | 420 | 280 | 12 | 435 | 400 | 23 |
Key words:
ptfe lined pipe fittings | ptfe lined tee | ptfe lined reducer | ptfe lined elbow | ptfe lined cross |
ptfe lined pipe and fittings | ptfe lined90degree elbow | ptfe lined 45 degrdd elbow | ptfe lined ECC reducer | ptfe lined CON reducer |
ptfe lined equal tee | ptfe lined reduce tee | ptfe lined unequal tee | ptfe lined pipe | ptfe lined fittings |
ptfe lined carbon steel pipe fittings | ptfe lined carbon steel tee | ptfe lined carbon steel reducer | ptfe lined carbon steel elbow | ptfe lined carbon steel cross |
PTFE pipe | PTFE lined pipe(Australia) | Resistant Stainless Steel Pipe | Resistant Steel Pipe | Carbon seamless steel pipe |
Anti Corrosion Pipe Fittings Lined | PTFE lining fittings | PTFE lined piping | straight tee | PTFE lined bends |
The chemical compatibility of LDPE and HDPE on this chart is tested at 20°C: and 50°C: for 7 days and 30 days (if applicable) with constant exposure.
LDPE & HDPE resistance listed by chemical | |
1.4-dioxane | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: shows some effect after 7 days. |
Acetaldehyde | LDPE / HDPE at 20°C: little or no damage after 30 days. HDPE at 50°C: shows some effect after 7 days. LDPE at 50°C: immediate damage may occur. |
Acetic Acid 5 % | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Acetic Acid, glacial 50% | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50 °C: immediate damage may occur. |
Acetone | LDPE / HDPE at 20°C-50°C: damage may occur. Not recommended for continuous use. |
Allyl Alcohol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Aluminum salts | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Amino acids | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Ammonia | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Ammonium carbonate saturated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Ammonium phosphate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Ammonium sulphate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Amyl chloride | HDPE at 20°C: shows some effect after 7 days. HDPE at 50°C & LDPE at 20°C-50°C: immediate damage may occur. Not recommended for continuous use. |
Aniline | LDPE / HDPE at 20°C: little or no damage after 30 days. HDPE at 50°C: shows some effect after 7 days. |
Benzene | LDPE / HDPE at 20°C-50°C: damage may occur. Not recommended for continuous use. |
Benzyl alcohol | LDPE / HDPE at 50°C: immediate damage may occur. HDPE at 20°C: shows some effect after 7 days. |
Boric acid | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Bromine | LDPE / HDPE at 50°C: immediate damage may occur. HDPE at 20°C: shows some effect after 7 days. |
Butyric acid | LDPE / HDPE at 50°C: immediate damage may occur. HDPE at 20°C: shows some effect after 7 days. |
Calcium chloride | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Calcium hydroxide saturated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Carbon tetrachloride | HDPE at 20°C: shows little or no damage after 30 days. LDPE at 20°C & HDPE at 50°C: show some effect after 7 days. LDPE at 50°C: not recommended. |
Chlorine 10% in water | LDPE / HDPE at 20°C: shows little or no damage after 30 days. LDPE at 50°C: shows damage and is not recommended. |
Chlorobenzene | Immediate damage may occur. Not recommended for continuous use. |
Chloroform | LDPE / HDPE at 20°C: show some effect after 7 days. LDPE / HDPE at 50°C: immediate damage may occur. Not recommended for continuous use. |
Chromic acid 10% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Chromic acid 50% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Citric acid 10% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Cresol | HDPE at 20°C: shows some effect after 7 days. LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage. Not recommended for continuous use. |
Cyclohexane | LDPE / HDPE at 50°C: immediate damage may occur. LDPE / HDPE at 20°C: show some effect after 7 days. |
Diethyl ketone | LDPE / HDPE at 20°C-50°C: damage may occur. Not recommended for continuous use. |
Dimethylsulfoxide | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Ethanol 95% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Ethyl acetate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Ethyl benzene | HDPE at 20°C: shows some effect after 7 days. LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage. Not recommended for continuous use. |
Ethylene glycol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Ethylene oxide | HDPE at 20°C: shows little or no damage after 30 days. LDPE at 20°C: and LDPE/ HDPE at 50°C: show some effect after 7 days. |
Ferric chloride | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Fluoride | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Fluorine | HDPE at 20°C: shows little or no damage after 30 days. LDPE at 20°C: shows some effect after 7 days. Not recommended at 50°C. |
Formaldehyde 10% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Formaldehyde 40% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Glycerol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hexane | HDPE at 20°C: shows little or no damage after 30 days continuous use. HDPE at 50 °C: shows some effect after 7 days. LDPE not recommended at any temperature. |
Hydrochloric acid 20% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hydrochloric acid 35% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hydrochloric acid 5% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hydrocyanic acid | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hydrofluoric acid | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hydrofluoric acid 4% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hydrofluoric acid 48% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hydrogen peroxide 3% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Hydrogen peroxide 30% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Isobutyl alcohol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Isopropyl alcohol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Kerosene | LDPE / HDPE at 20°C: show some effect after 7 days. LDPE / HDPE not recommended at 50°C, as immediate damage may occur. |
Lactic Acid 10 % | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Lactic Acid 90 % | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Lead acetate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Methanol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Methyl ethyl ketone | Immediate damage may occur. Not recommended for continuous use. |
Methyl propyl ketone | HDPE at 20°C: shows some effect after 7 days. LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur. Not recommended for continuous use. |
Methylene chloride | HDPE at 20°C: shows some effect after 7 days. LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur. Not recommended for continuous use. |
Mineral oil | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: may show immediate damage and is not recommended. |
n-amyl acetate | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: shows some effect after 7 days or constant exposure. |
n-butyl alcohol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Nitric acid 50 % | LDPE at 20°C: shows little or damage after 30 days. HDPE at 20°C & LDPE at 50°C: show effect after 7 days. HDPE at 50°C: shows immediate damage and is not recommended. |
Nitric acid 70 % | LDPE / HDPE at 20°C: show some effect after 7 days. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
n-octane | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Oleic acid | HDPE at 20°C-50°C: little or no damage after 30 days. LDPE at 20°C-50°C: shows immediate damage and is not recommended. |
Oxalic acid | LDPE at 20°C: shows some effect after 7 days. HDPE at 20°C and LDPE / HDPE at 50°C: shows little/ no damage after 30 days. |
Ozone | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
Perchloric acid | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
Perchloric ethylene | LDPE / HDPE at 20°C-50°C: show immediate damage. Not recommended. |
Phenol | LDPE / HDPE at 20°C-50°C: show immediate damage. Not recommended. |
Phosphoric acid 10% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Phosphoric acid 85% | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: shows immediate damage and is not recommended. |
Phosphorous trichloride | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: has no data available. HDPE at 50°C: shows some effect after 7 days. |
Potassium carbonate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Potassium hydroxide 5 % | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Potassium hydroxide concentrated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Potassium permanganate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Propylene glycol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Pyridine | Immediate damage may occur. Not recommended for continuous use. |
Salicylic acid, saturated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Silver acetate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Silver nitrate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sodium carbonate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sodium chloride, saturated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sodium dichromate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sodium hydroxide 1% | LDPE at 20°C-50°C: shows little or no damage after 30 days. HDPE at 20°C-50°C: shows some effect after 7 days. |
Sodium hydroxide 50% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sodium hypochlorite 15% | HDPE at 20°C-50°C: little or no damage after 30 days. LDPE at 20°C: is suitable but at 50°C: shows some effect after 7 days. |
Sodium nitrate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sodium sulphate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sucrose | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sulfuric acid 20% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sulfuric acid 6% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sulfuric acid 60% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Sulfuric acid 98% | LDPE at 20°C-50°C: shows little or no damage after 30 days. HDPE at 20°C: shows effect after 7 days. Not recommended for use at 50°C. |
Tannic acid | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Tetrahydrofuran | LDPE / HDPE at 20°C: show some effect after 7 day of constant exposure. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
Toluene | LDPE at 20°C: show some effect after 7 day of constant exposure. HDPE at 20°C-50°C & LDPE at 50°C: show immediate damage. Not recommended. |
Trichloracetic acid | LDPE / HDPE at 20°C: show some effect after 7 day of constant exposure. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
Trichlorethane | Immediate damage may occur. Not recommended for continuous use. |
Turpentine oil | LDPE / HDPE at 20°C: show some effect after 7 days. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
Urea | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
Xylene | HDPE at 20°C: shows some effect after 7 day of constant exposure. LDPE at 20-50°C and HDPE at 50°C: show immediate damage. Not recommended. |
Zinc chloride | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |