Customizing Underground Chemical Storage Tank 100mt-150mt

Product Details
Customization: Available
After-sales Service: 24hours
Warranty: 24months
Shipping & Policy
Shipping Cost: Contact the supplier about freight and estimated delivery time.
Payment Methods:
visa mastercard discover JCB diners club american express T/T
PIX SPEI OXXO PSE OZOW
  Support payments in USD
Secure payments: Every payment you make on Made-in-China.com is protected by the platform.
Refund policy: Claim a refund if your order doesn't ship, is missing, or arrives with product issues.
Manufacturer/Factory, Trading Company, Group Corporation
Secured Trading Service
Diamond Member Since 2015

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Cooperated with Fortune 500
This supplier has Cooperated with Fortune 500 companies
Customization from Designs
The supplier provides design based customization services
ODM Services
The supplier provides ODM services
OEM Services
The supplier provides OEM services for popular brands
to see all verified strength labels (11)
  • Customizing Underground Chemical Storage Tank 100mt-150mt
  • Customizing Underground Chemical Storage Tank 100mt-150mt
  • Customizing Underground Chemical Storage Tank 100mt-150mt
  • Customizing Underground Chemical Storage Tank 100mt-150mt
  • Customizing Underground Chemical Storage Tank 100mt-150mt
  • Customizing Underground Chemical Storage Tank 100mt-150mt
Find Similar Products

Basic Info.

Model NO.
Chemical Storage Tank
Condition
New
Customized
Customized
Tank Marerial
Metal Tank
Type
Horizontal / Vertical
Storage Objects
Liquid
Materical
Q235A + PE (Plastic )16mm -22mm
Type H
Horizontal / Vertical
Shell Thickness
6mm/8mm/10mm/12mm
Storage
Hydrochloric Acid, Sulphuric Acid...
Transport Package
Nil
Specification
OEM
Trademark
Dong Run Ze
Origin
China
HS Code
73090000
Production Capacity
8000

Packaging & Delivery

Package Size
1200.00cm * 350.00cm * 380.00cm
Package Gross Weight
12000.000kg

Product Description


Customizing Underground Chemical Storage Tank 100MT-150MT
Used to contain: HCl (max 35%), NaOH (max 50%), NaCLO (max 10%), PAC (max 17%), H2SO4 etc 



Horizontal / Vertical Storage HCL Acid Tanks Steel Lined LDPE 120000 Liters 
For Storage Bleach, Hydrochloric Acid, Ferric Chloride, Oilfield Chemicals, Corrosive Wastes And Other Hazardous Cargoes. 
Steel ( 6 mm -8mm ) Lined PE Plastic 7042 (16mm - 25 mm ) storage tank
 Customizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mt

Underground Gasoline Fuel Oil Storage Tank

 Customizing Underground Chemical Storage Tank 100mt-150mt

Horizontal  Storage HCL Acid Tanks Steel Lined LDPE  120000 Liters 

For Storage  Bleach, Hydrochloric Acid, Ferric Chloride, Oilfield Chemicals, Corrosive Wastes And Other Hazardous Cargoes.

      Customizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mtCustomizing Underground Chemical Storage Tank 100mt-150mt    Steel ( 6 mm -8mm ) Lined PE - Plastic 7042  (16mm - 20 mm ) storage tank

storage hydrochloride, hydrogen chlorate, sodium hydroxide,acrylic 

acetic acid, glacial acetic acid, hydrogen peroxide 

Propionic acid, ammonia,NH3·H2O 

other tanks

                                                                         

       water tank        stainless steel tank /water pump/ High pressure squirt gun
       steel option        Q235/Q345/ 16 manganese steel/SS201/SS304 /SS316 alummin alloy tanker
       acids tanker        steel lined plastic for water/alcohol/ethanol acid, alkaline and salt HCL, NaOH ,NaCIO Sodium Hypochlorite NaCIO /hydrofluoric acid HF/CAUSTIC SODA alummin nitric acid
       oil/petrol,Fuel diesel/LPG/LNG        steel tank with oil pump/ gun fuel truck nozzle
       asphalt/bitumen/crude oil tanker/ AN ammonium methana Alcohol        burner/steam heating and insulation system ,pump option

                                                                                                                                                                                    



Vertical type PE  Plastic  tank
Capaicty Shell length Total length Diameter Weight  Shell thickness EXW Price
1m3  750 mm 930 mm 1300 mm 95(KG) 15 mm $1355~$2060
2m3 1800 mm 1980 mm 1300 mm 150(KG) 15 mm $1565~$2260
5m3 1100 mm 1400 mm 2400 mm 260(KG) 15 mm $1880~$2560
10m3 2200 mm 2500 mm 2400 mm 500(KG) 20 mm $2508~$3560
15m3 3300 mm 3600 mm 2400 mm 680(KG) 20 mm $3850~$5560
20m3 4400 mm 4700 mm 2400 mm 850(KG) 22 mm $5480~$7180
30m3 4400 mm 5040 mm 3000 mm 1350(KG) 25 mm $6490~$8190
40m3 4900 mm 5500 mm 3450 mm 2000(KG) 32 mm $6860~$8560
50m3 6000 mm 6600 mm 3450 mm 2300(KG) 32 mm $11520~$13920

5 cbm/m3
Q235A 5mm+ PE  (Plastic )16mm US$7,200.00
10 m3 Q235A 5mm+PE16mm US$9,200.00
20 m3 Q235A 5mm+PE16mm US$11,200.00
30 Q235A 6mm+PE16mm US$13,200.00
40 Q235A 6mm+PE16mm US$15,200.00
50 Q235A 6mm+PE16mm US$17,200.00
60 Q235A 6mm+PE16mm US$19,200.00
70 Q235A 6mm+PE16mm US$21,200.00
80 Q235A 8mm+PE16mm US$23,200.00
90 Q235A 8mm+PE16mm US$25,200.00
100 Q235A 8mm+PE16mm US$27,200.00
110 Q235A 8mm+PE16mm US$29,200.00
120 Q235A 8mm+PE16mm US$30,800.00
130 Q235A 8mm+PE16mm US$32,400.00
135 Q235A 8mm+PE16mm US$34,400.00

                                                                                                       

manufacturer, supplier and exporter of Acid Storage Tank in China. Storage Tanks are widely used for storing chemicals and acids and can be availed in various models such as horizontal and vertical. These tanks are equipped with best quality stainless steel material and mild steel, extensively used in various industries - such as pharmaceutical, sugar, food and dairy. This storage tank is widely in demand and accepted by our clients.

Being a quality centric organization, our product line includes Plastic Storage Tank, Chemical Storage Tank, Horizontal Storage tank, Bottom Conical Storage Tank and many more. The manufactured range of Acid Storage Tanks is available to the clients in different sizes using high quality design and welding standards. Storage tanks are mostly appropriate for over ground and underground installations and can be used to store acids in safe and secure way. 

 we cater to the bulk requirements of the clients and strive to offer the best quality products manufactured in compliance with international standards. We have been able to mark our strong foothold as one the leading Manufacturer of Acid Storage Tanks from China

LDPE & HDPE  polyethylene  resistance listed by chemical 
1.4-dioxane LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows 
some effect after 7 days of constant exposure. 
Acetaldehyde LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows 
some effect after 7 days of constant exposure. LDPE - immediate damage may occur. 
Acetic Acid 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Acetic Acid, glacial 50% LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50 C° - 
immediate damage may occur. 
Acetone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use. 
Allyl Alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Aluminum salts LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Amino acids LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Ammonia LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Ammonium carbonate, 
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Ammonium phosphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Ammonium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Amyl chloride HDPE at 20C° shows some effect after 7 days of constant exposure. HDPE at 50C° and LDPE at 20C°-50C° - 
immediate damage may occur. Not recommended for continuous use. 
Aniline LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows 
some effect after 7 days of constant exposure. 
Benzene LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use. 
Benzyl alcohol LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of 
constant exposure. 
Boric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Bromine LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of 
constant exposure. 
Butyric acid LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of 
constant exposure. 
Calcium chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Calcium hydroxide 
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Calcium sulphate No data is available at this time. 
Carbon tetrachloride HDPE at 20C° shows little or no damage after 30 days. LDPE at 20C° and HDPE at 50C° show some effect 
after 7 days of constant exposure. LDPE at 50C° not recommended. 
Chlorobenzene Immediate damage may occur. Not recommended for continuous use. 
Chloroform HDPE and LDPE at 20C° show some effect after 7 days. At -50C° - immediate damage may occur. Not 
recommended for continuous use. 
Chlorine 10% in water HDPE and LDPE at 20C° shows little or no damage after 30 days. LDPE at 50C° shows damage and is not 
recommended. 
Chromic acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Chromic acid 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Citric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Cresol HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate 
damage and are not recommended for continuous use. 
Cyclohexane LDPE and HDPE at 50C° - immediate damage may occur. HDPE and LDPE at 20C° show some effect after 7 
days of constant exposure. 
Diethyl ketone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use. 
Dimethylsulfoxide LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Ethanol 95% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. Ethyl acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Ethyl benzene HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate 
damage and are not recommended for continuous use. 
Ethylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Ethylene oxide HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° and LDPE/ HDPE 
at 50C° show some effect after 7 days. 
Ferric chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Fluoride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Fluorine HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° shows some effect 
after 7 days. Neither HDPE or LDPE are recommended at 50C°. 
Formaldehyde 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Formaldehyde 40% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Glycerol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Heating oil No further data is available at this time. 
Hexane HDPE at 20C° shows little or no damage after 30 days continuous use and at 50 C° shows some effect after 7 
days. LDPE not recommended at any temperature. 
Hydrochloric acid 5% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Hydrochloric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Hydrochloric acid 35% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Hydrocyanic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Hydrofluoric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Hydrofluoric acid 4% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Hydrofluoric acid 48% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Hydrogen peroxide 3% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Hydrogen peroxide 30% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Isobutyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Isopropyl acetate No data is available at this time. 
Isopropyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Kerosene LDPE and HDPE at 20C° show some effect after 7 days. HDPE and LDPE not recommended at 50C°, as 
immediate damage may occur. 
Lactic Acid 10 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Lactic Acid 90 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Lead acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Metallic salts, dissolved No data is available at this time. 
Methanoic acid 100% No data is available at this time. 
Methanol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Methyl ethyl ketone Immediate damage may occur. Not recommended for continuous use. 
Methyl propyl ketone HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage 
may occur. Not recommended for continuous use. 
Methylene chloride HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage 
may occur. Not recommended for continuous use. 
Mineral oil LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° may 
show immediate damage and is not recommended. 
n-amyl acetate LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows 
some effect after 7 days or constant exposure. 
n-butyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
n-octane LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Nitric acid 50 % LDPE at 20C° shows little or damage after 30 days. HDPE at 20C° and LDPE at 50C° show effect after 7 days. 
HDPE at 50C° shows immediate damage and is not recommended. 
Nitric acid 70 % HDPE and LDPE at 20C° show some effect after 7 days. Both at 50C° show immediate damage and are not 
recommended. 
Oleic acid HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C°-50C° shows 
immediate damage and is not recommended. 
Oxalic acid LDPE at 20C° shows some effect after 7 days. HDPE at 20C° and both HDPE and LDPE at 50C° show little or 
no damage after 30 days. 
Ozone HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at 
50C° show immediate damage and are not recommended. 
Perchloric acid HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at 50C° show immediate damage and are not recommended. 
Perchloric ethylene HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended. 
Phenol HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended. 
Phosphoric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Phosphoric acid 85% HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows 
immediate damage and is not recommended. 
Phosphorous trichloride HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° has no 
data available. HDPE at 50C° shows some effect after 7 days. 
Potassium acetate No data is available at this time. 
Potassium bromide No data is available at this time. 
Potassium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Potassium hydroxide 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Potassium hydroxide 
concentrated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Potassium permanganate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Propylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Pyridine Immediate damage may occur. Not recommended for continuous use. 
Salicylic acid, saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Silver acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Silver nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sodium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sodium chloride, 
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sodium dichromate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sodium hydroxide 1% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C°-50C° shows 
some effect after 7 days. 
Sodium hydroxide 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sodium hypochlorite 15% HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C° is suitable but 
at 50C° shows some effect after 7 days. 
Sodium nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sodium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sucrose LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sulphide No additional information is available at this time. 
Sulfuric acid 6% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sulfuric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sulfuric acid 60% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Sulfuric acid 98% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C° shoes effect 
after 7 days and is not recommended for use at 50C°. 
Tannic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Tetrahydrofuran HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show 
immediate damage and are not recommended. 
Toluene LDPE at 20C° show some effect after 7 day of constant exposure. HDPE at 20C°-50C° and LDPE at 50C° 
show immediate damage and are not recommended. 
Trichloracetic acid HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show 
immediate damage and are not recommended. 
Trichlorethane Immediate damage may occur. Not recommended for continuous use. 
Turpentine oil HDPE and LDPE at 20C° show some effect after 7 day of constant exposure. HDPE and LDPE at 50C° show 
immediate damage and are not recommended. 
Urea LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. 
Xylene HDPE at 20C° shows some effect after 7 day of constant exposure. LDPE at 20-50C° and HDPE at 50C° show 
immediate damage and are not recommended. 
Zinc chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now