Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory

Product Details
Customization: Available
After-sales Service: 24
Warranty: 24
Manufacturer/Factory, Trading Company, Group Corporation
Diamond Member Since 2015

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Cooperated with Fortune 500
This supplier has Cooperated with Fortune 500 companies
Customization from Designs
The supplier provides design based customization services
ODM Services
The supplier provides ODM services
OEM Services
The supplier provides OEM services for popular brands
to see all verified strength labels (11)
  • Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
  • Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
  • Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
  • Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
  • Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
  • Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
Find Similar Products
  • Overview
  • Certifications
  • Packaging & Shipping
Overview

Basic Info.

Model NO.
Steel Lined PE Pipe
Condition
New
Customized
Customized
Tank Marerial
Metal Tank
Type
Horizontal / Vertical
Storage Objects
Liquid, Gas
Materical
Q235A + PE (Plastic )16mm -22mm
Type H
Horizontal / Vertical
Transport Package
Nil
Specification
OEM
Trademark
Dong Run Ze
Origin
China
HS Code
73090000
Production Capacity
8000

Product Description

Anticorrosive Steel Lined Plastic PTFE ,LLDPE  Pipe Use for  Sulfuric Acid Hydrochloric Acid  HCL, NaOH, NaCLO,
Steel lined piping with tetrafluoride
Molded piping with tetrafluoride
Anticorrosive pipeline resistant to high temperature and negative pressure
Chemical pipeline


Metal cans Steel-Lined Plastic Square Tank, Electrolytic Tank, Pickling Tank  Acid Containment Vessels Custom Made Rotationally Molded Linear Resins LLDPE
Custermizing Checmial Acid Storage Tank 60 m3 Steel Lined LLDPE  Tank Used to Contain: HCl (max 35%) , Naoh (max 50%) , Naclo (max 10%) , PAC (max 17%) ,H2so4  

Used to contain: HCl (max 35%), NaOH (max 50%), NaCLO (max 10%), PAC (max 17%), H2SO4 etc 


 Media (density) : (1155 Kg/m3), Hydrochloric Acid (1150 Kg/m3), Sulfate, Nitrate (1152 Kg/m3), Phosphate (1151 Kg/m3), Hydrofluoric Acid (1132 Kg/m3), Battery Fluid (1135 Kg/m3), Chloride (1135 Kg/m3), Ferric Chloride Solution (1130 Kg/m3), Sodium Hypochlorite (1130 Kg/m3), Sulfurous Acid (1030 Kg/m3)

processing/storing; aluminum sulfate, ammonium sulfate, calcium chloride, ethylene glycol, ferric chloride, ferric sulfate, ferrous sulfate, hydrochloric acid, hydrofluoric acid, hydrofluosilicic acid, hydrogen peroxide, magnesium chloride, phosphoric acid, polymers, potassium hydroxide, or just plain water and we'll design the vessel(s) you require.

Horizontal / Vertical Storage HCL Acid Tanks Steel Lined LDPE 120000 Liters 
For Storage Bleach, Hydrochloric Acid, Ferric Chloride, Oilfield Chemicals, Corrosive Wastes And Other Hazardous Cargoes. 
Steel ( 6 mm -8mm ) Lined PE Plastic 7042 (16mm - 25 mm ) storage tank

Detail Picture
Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory

Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
Steel Lined PE (PTFE / PP /PO) Pipe for Chemical FactorySteel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
01.Carefully selected seamless steel pipe

02 .Steel pipe Weld Flange and Polishing

03 .Steel pipe Sandblasting 

Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory

04 .Steel pipe Lined PE

Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
05 .Steel pipe Cooling,Primer, Topcoat Paint Anti rust


Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory
 

Specification General PTFE thickness and negative pressure-resistance The thickness of PTFE wall required to resist-0.1MPA pressure when the temperature is less than 120degree,
DN25 2mm -0.08Mpa 3mm(L≤3000mm)
DN32 2mm -0.075Mpa 3mm(L≤3000mm)
DN40 2.5mm -0.075Mpa 4mm(L≤3000mm)
DN50 2.5mm -0.06Mpa 5mm(L≤3000mm)
DN65 2.5mm -0.05Mpa 8mm(L≤1000mm)
DN80 3mm -0.05Mpa 10mm(L≤1000mm)
DN100 3mm -0.04Mpa 13mm(L≤1000mm)
DN125 4mm -0.03Mpa 13mm(L≤1000mm)
DN150 4mm -0.025Mpa 13mm(L≤1000mm)
DN200 5mm -0.02Mpa 15mm(L≤1000mm)
Specifications:
Nominal Diameter (mm/in. ): DN15-DN600 (NPS 1/2-NPS 24)
Operating temperature: -20-180 degree
Operating pressure: -0.09MPa-1.6MPa (-0.9bar-16bar)
Pipe: Seamless steel.
Flange: ASME B16.5 Class 150 Flange options: HG, GB, JB, JIS, BS, DIN, ANSI, ASTM
Special pieces of specific or non standard size can be manufactured on request.

Carbon steel 45/90degree ptfe lined elbow
Operating temperature: -20-180
Operating pressure: -0.09MPa-1.6MPa



Carbon steel 45/90degree ptfe lined elbow
1. Positive pressure: It shall adopt steel components according to different technical requirements, and the thickness of PTFE wall shall be over 2mm. If the temperature is less than 100 degree, the production length shall be less than 6m; And if the temperature exceeds 100 degree, the length shall be less than 3m.
2. Negative pressure: Design according to different ambient conditions of the users
PTFE lined 90° elbow           Unit mm
Nominal diameter Specification of balled iron T Raised face A Central height C1 Inside diameter D1 PTFE thickness out side diameter of flange D Diameter of bolt circle K Thickness of flange C
DN(mm) NPS(inch)
DN15 1/2 34 40 80 15 5 90 65 11
DN20 3/4 38 45 90 18 5 100 75 11
DN25 1 42 60 92 22 5 110 85 12
DN32 1 1/4 48 70 100 28 5 130 100 13
DN40 1 1/2 57 80 112 38 5 140 110 14
DN50 2 68 95 117 48 5 155 125 14
DN65 2 1/2 89 115 135 63 8 175 145 16
DN80 3 108 130 150 78 8 190 160 16
DN100 4 114 150 150 87 8 210 180 18
DN125 5 140 180 190 110 8 240 210 20
DN150 6 168 205 230 135 10 275 240 20
DN200 8 219 260 305 180 10 330 295 20
DN250 10 273 315 380 230 12 385 350 23
DN300 12 325 365 420 280 12 435 400 23

 

Key words:

ptfe lined pipe fittings ptfe lined tee ptfe lined reducer ptfe lined elbow ptfe lined cross
ptfe lined pipe and fittings ptfe lined90degree elbow ptfe lined 45 degrdd elbow ptfe lined ECC reducer ptfe lined CON reducer
ptfe lined equal tee ptfe lined reduce tee ptfe lined unequal tee ptfe lined pipe ptfe lined fittings
ptfe lined carbon steel pipe fittings ptfe lined carbon steel tee ptfe lined carbon steel reducer ptfe lined carbon steel elbow ptfe lined carbon steel cross
PTFE pipe  PTFE lined pipe(Australia)    Resistant Stainless Steel Pipe Resistant Steel Pipe Carbon seamless steel pipe
Anti Corrosion Pipe Fittings Lined PTFE lining fittings  PTFE lined piping straight tee PTFE lined bends



Certifications

Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory

Packaging & Shipping

Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory



Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory

 


Steel Lined PE (PTFE / PP /PO) Pipe for Chemical Factory

 

 








Rotationally Molded LLDPE TANK
 chemical resistance of LLDPE   
 
 tictrucks.en.made-in-china.com   

LDPE / HDPE Chemical Resistance Chart 

The chemical compatibility of LDPE and HDPE on this chart is tested at 20°C: and 50°C: for 7 days and 30 days (if applicable) with constant exposure.

LDPE & HDPE resistance listed by chemical
1.4-dioxane LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows some effect after 7 days.
Acetaldehyde LDPE / HDPE at 20°C: little or no damage after 30 days.
HDPE at 50°C: shows some effect after 7 days.
LDPE at 50°C: immediate damage may occur.
Acetic Acid 5 % LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Acetic Acid, glacial 50% LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50 °C: immediate damage may occur.
Acetone LDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
Allyl Alcohol LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Aluminum salts LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Amino acids LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonia LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium carbonate saturated LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium phosphate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium sulphate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Amyl chloride HDPE at 20°C: shows some effect after 7 days.
HDPE at 50°C & LDPE at 20°C-50°C: immediate damage may occur.
Not recommended for continuous use.
Aniline LDPE / HDPE at 20°C: little or no damage after 30 days.
HDPE at 50°C: shows some effect after 7 days.
Benzene LDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
Benzyl alcohol LDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Boric acid LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Bromine LDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Butyric acid LDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Calcium chloride LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Calcium hydroxide saturated LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Carbon tetrachloride HDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C & HDPE at 50°C: show some effect after 7 days.
LDPE at 50°C: not recommended.
Chlorine 10% in water LDPE / HDPE at 20°C: shows little or no damage after 30 days.
LDPE at 50°C: shows damage and is not recommended.
Chlorobenzene Immediate damage may occur.
Not recommended for continuous use.
Chloroform LDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: immediate damage may occur.
Not recommended for continuous use.
Chromic acid 10% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Chromic acid 50% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Citric acid 10% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Cresol HDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage.
Not recommended for continuous use.
Cyclohexane LDPE / HDPE at 50°C: immediate damage may occur.
LDPE / HDPE at 20°C: show some effect after 7 days.
Diethyl ketone LDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
Dimethylsulfoxide LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethanol 95% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethyl acetate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethyl benzene HDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage.
Not recommended for continuous use.
Ethylene glycol LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethylene oxide HDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C: and LDPE/ HDPE at 50°C: show some effect after 7 days.
Ferric chloride LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Fluoride LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Fluorine HDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C: shows some effect after 7 days.
Not recommended at 50°C.
Formaldehyde 10% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Formaldehyde 40% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Glycerol LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hexane HDPE at 20°C: shows little or no damage after 30 days continuous use.
HDPE at 50 °C: shows some effect after 7 days.
LDPE not recommended at any temperature.
Hydrochloric acid 20% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrochloric acid 35% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrochloric acid 5% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrocyanic acid LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acid LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acid 4% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acid 48% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrogen peroxide 3% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrogen peroxide 30% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Isobutyl alcohol LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Isopropyl alcohol LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Kerosene LDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE not recommended at 50°C, as immediate damage may occur.
Lactic Acid 10 % LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Lactic Acid 90 % LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Lead acetate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Methanol LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Methyl ethyl ketone Immediate damage may occur.
Not recommended for continuous use.
Methyl propyl ketone HDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur.
Not recommended for continuous use.
Methylene chloride HDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur.
Not recommended for continuous use.
Mineral oil LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: may show immediate damage and is not recommended.
n-amyl acetate LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows some effect after 7 days or constant exposure.
n-butyl alcohol LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Nitric acid 50 % LDPE at 20°C: shows little or damage after 30 days.
HDPE at 20°C & LDPE at 50°C: show effect after 7 days.
HDPE at 50°C: shows immediate damage and is not recommended.
Nitric acid 70 % LDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
n-octane LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Oleic acid HDPE at 20°C-50°C: little or no damage after 30 days.
LDPE at 20°C-50°C: shows immediate damage and is not recommended.
Oxalic acid LDPE at 20°C: shows some effect after 7 days.
HDPE at 20°C and LDPE / HDPE at 50°C: shows little/ no damage after 30 days.
Ozone LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Perchloric acid LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Perchloric ethylene LDPE / HDPE at 20°C-50°C: show immediate damage.
Not recommended.
Phenol LDPE / HDPE at 20°C-50°C: show immediate damage.
Not recommended.
Phosphoric acid 10% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Phosphoric acid 85% LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows immediate damage and is not recommended.
Phosphorous trichloride LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: has no data available. HDPE at 50°C: shows some effect after 7 days.
Potassium carbonate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium hydroxide 5 % LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium hydroxide concentrated LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium permanganate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Propylene glycol LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Pyridine Immediate damage may occur.
Not recommended for continuous use.
Salicylic acid, saturated LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Silver acetate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Silver nitrate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium carbonate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium chloride, saturated LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium dichromate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium hydroxide 1% LDPE at 20°C-50°C: shows little or no damage after 30 days.
HDPE at 20°C-50°C: shows some effect after 7 days.
Sodium hydroxide 50% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium hypochlorite 15% HDPE at 20°C-50°C: little or no damage after 30 days.
LDPE at 20°C: is suitable
 but at 50°C: shows some effect after 7 days.
Sodium nitrate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium sulphate LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sucrose LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 20% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 6% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 60% LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 98% LDPE at 20°C-50°C: shows little or no damage after 30 days.
HDPE at 20°C: shows effect after 7 days.
Not recommended for use at 50°C.
Tannic acid LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Tetrahydrofuran LDPE / HDPE at 20°C: show some effect after 7 day of constant exposure.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Toluene LDPE at 20°C: show some effect after 7 day of constant exposure.
HDPE at 20°C-50°C & LDPE at 50°C: show immediate damage.
Not recommended.
Trichloracetic acid LDPE / HDPE at 20°C: show some effect after 7 day of constant exposure.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Trichlorethane Immediate damage may occur.
Not recommended for continuous use.
Turpentine oil LDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Urea LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Xylene HDPE at 20°C: shows some effect after 7 day of constant exposure.
LDPE at 20-50°C and HDPE at 50°C: show immediate damage.
Not recommended.
Zinc chloride LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier